200 - 40,000 kilogram
40,001 - 999,999 kilogram
group nameRTV-2 silicone rubber for molds making
Min Order200 kilogram
brand nameHong Ye silicone rubber
modelRTV 625#
payment methodT/T, L/C, Westem Union
update timeTue, 05 Nov 2013 13:19:11 GMT
Colors white/any
Hardness 18 A°~40A°(Adjustable)
Application size of mold Adjustable
Recommend operation way pouring/brushing
Retractility(%) ≤0.25
Certifications ISO,FDA,RoHS
Shelf life 12 month
Packing 25kg/pail
Payment T/T
Transport By sea or air
Min Order200 kilogram
Silicone Kit For Mold Making application:
Silicone Kit For Mold Making are suitable for mold masters for molding with polyester resin, epoxy resin, urethane foam, wax, plaster, and low-melt-point metal alloys. These RTV rubber compounds allow accurate reproduction of the shape of the original. They are easy to use and are thus used widely in industrial applications, as well as by hobbyists looking to create the perfect replica.
Silicone Kit For Mold Making description
A. Workability
The base compound and curing agent are mixed and then poured into the mold to create a silicone rubber mold quickly. Workable time and cure time can be adjusted.
B. Mold-releasability
The cured rubber releases easily from the mold, so mold-release agents (soapy water, wax, etc.) are unnecessary.
C.Dimensional stability
These rubbers offer good dimensional stability, with little shrinkage.
D. Flowability
They have excellent flowability, so the original form is reproduced accurately. This includes even intricate shapes and details such as fingerprints and wood grain.
E.Heat and chemical resistance
These rubbers have outstanding resistance to heat and chemicals.
F.Deep-section curability
Moldmaking RTV silicone rubber compound cures uniformly throughout the mold, regardless of thickness
G.Non-exothermic
No heat is generated during curing, meaning no adverse effects to the original.
3.Frequently asked questions of Silicone Kit For Mold Making
Why is the silicon mold oily?
The molding silicone rubber itself doesn’t contain any oil, so it won’t be oily. If the mold is oily, it may be because you add the compound silicone oil( the compound of silicon oil and white oil).
For getting further information about RTV-2 silicone rubber, PLS contact with