pad printing silicon equivalent to Dow-corning and wacker

FOB Price
  • US $18.88

    100 - 40,000 kilogram

  • US $8.99

    40,001 - 999,999 kilogram

  • group nameAddition cure silicone rubber

  • Min Order100 kilogram

  • brand nameHong Ye silicone rubber

  • modelHY-918

  • payment methodT/T, L/C, Westem Union

  • update timeFri, 08 Nov 2013 18:35:55 GMT

Paramtents

  • Certifications RoHS.MSDS.SGS ISO9001:2000

  • MOQ 100kgs

  • HS code 39100000

  • feature liquid

  • color any

  • mix ratio 1:1/9:1

  • materials silicone rubber

  • Place China

  • model 9 series

  • brand hongye silicone

Packging & Delivery

  • Min Order100 kilogram

Briefing

pad printing silicon rubber:
1. resistance to deformation, high-temperature
2. high printing times
3. good aging resistance

Detailed

pad printing silicon equivalent to Dow-corning and wacker  

 

is mainly use for printing irregular patterns of plastic toys, electroplating toys and trade makers . 

Pad printing silicone rubber as a carrier which transfer patterns on the steel plate to the toys products surface.

 

 pad printing silicon equivalent to Dow-corning and wacker Features:

 

Pad printing silicone rubber with high print times and abrasion resistance. Pad printing silicone rubber has good printing effects, permanent and durable. We can provide all kinds of color and our catalyst is free.  

FAQ:Why the pad printing silicon rubber can not transfer the printing pattern well?

It is normal phenomena that every two out of ten products have this problem if the plastic toys are not spray painted. As in the production process, mold release agent will be sprayed onto the surface of the steel plate for each one dozen products, and there will be some mold release agent left on the surface of the first one or two product. Please use Tianna water or face-clean water to clean the products before used for pad printing.

 

 Technical Datesheets of  pad printing silicon equivalent to Dow-corning and wacker

 

 Special silicone products for pad printing    

Model

 

901#

902#

912#

916#

918#

928#

Appearance

 

Red

white

Yellow

green

Red

white

Yellow

green

Red

white

Yellow

green

Red

white

Yellow

green

Red

white

Yellow

green

 

Red

white

 

 

Curing type

 

Condensation cure

 

Condensation

cure

Condensa-

tion cure

Condensa-

tion cure

Condensa-tion cure

Addition

cure

Mixing proportion

Of curing agent

2-3%

2-3%

2-3%

2-3%

2-3%

9:1

Operating time

(hours)

0.5

0.5

0.5

0.5

0.5

0.5

Curing time

(hours)

3-4

  3-4

  3-4

   3-4

   3-4

  3-4

 Hardness

(A°)

20-25

26-30

26-30

20-22

26-30

28-30

 Viscosity

(cs)

29000-34000

29000-34000

29000-35000

29000-35000

28000-34000

29000-35000

 Tensile-

 strength

( kgf /cm)

≥30

≥32

≥35

≥35

≥36

≥38

Tear-strength

( kgf /cm)

≥18

≥22

≥24

≥24

≥26

≥28

Elongation-

  break

  ( % )

≥360

≥380

≥410

≥420

≥420

≥450

Retractility

 (%)

≤0.3

≤0.3

≤0.3

≤0.3

≤0.3

≤0.15

Usage

 

Pad printing

only

Pad

printing only

Pad printing only

Pad printing only

Pad printing only

Pad 

printing 

only

 

 

pad printing silicon equivalent to Dow-corning and wacker

 

The normal proportion between the  pad printing silicon equivalent to Dow-corning and wackerand the silicone oil depends on the requirements of the customers. If pattern with big area to be printed, a soft silicon pad is needed and the amount of silicone oil is increased. Contrarily, if a silicon pad with high hardness is needed, the silicone oil should be added less or not . The hardness of general pad printing silicone rubber is approximate of 15A°~-25 A°; if too much silicone oil is added, the silicon pad is so soft that the printing times is limited, the molecular weight of the silicon will be damaged by the silicone oil no matter how superior quality the silicon is, thereby bringing about abrasion intolerance, solvent intolerance and ageing. 

 

 

 Need any help on pad printing silicon equivalent to Dow-corning and wacker, please feel free to contact Ms Annie :
Tel: 0086-0755-89948294    
Mob:0086-0755-18938861891
E-mail: hyjx(at)szrl(dot)net   
skype: annie2012a

Nearest port for product export
Shenzhen, Guangzhou, Xiamen, Shanghai
Delivery clauses under the trade mode
FOB, CFR, CIF
Acceptable payment methods
T/T, L/C, Westem Union
Export mode
Export through agents
Contact Suppliers

Follow this Suppliers