Paramtents

  • Color translucent silicone rubber

  • Hardness(shore A) 42±2

  • Mix ratio(A:B) 1:1/10:1

  • Viscocity Part A (mPa.s) 30000±2000

  • Viscocity Part B (mPa.s) 6000±500

  • Tensile strength (kgf/cm2) 65±5

  • Tear-strength (kN/m) 16±2

  • Elongation(%) 450±50

  • Pot life/working time (mins) 30-40

  • Curing time/setting time (hrs) 3-4hrs(25℃)10-20mins(60℃)

Packging & Delivery

  • Min Order100 kilogram

Briefing

platinum catalyst addition cure silicone rubber features:
rtv silicone with fine quality,
favorible resilience,
transparent

Detailed

 

 

 Description of  platinum catalyst addition cure silicone rubber

 

platinum catalyst addition cure silicone rubber is a kind of FDA grade silicone , generally named two-components silicone rubber with translucent appearance, Part A and part B mixing in 1:1 .Its suitable for molds making application.

 

 

 

Applications of  platinum catalyst addition cure silicone rubber

 

Platinum cure silicone rubber mainly used for making concrete stones, wax molds, PU molds, resin molds, gypsum casting, candle molding and chocolate , candy and any other food product molds making 

 

 platinum catalyst addition cure silicone rubber

 

Advantage of platinum catalyst addition cure silicone rubber

 

1)Non- shrinkage (less than 0.1% )

 

2)High tensile and tear strength with high copy times

 

3)Exceptional fluidity and good operability (mixing ratio at 1:1 )

 

4)High temperature resistant in 250 Centigrade 

 

 

 

Operation instruction of platinum catalyst addition cure silicone rubber

 

Step One: Take 100g of part A and 100g of part B and mix in 1:1 and mix the two part evenly.

 

 

 

Step Two: vacuum pumping

 

Without exception, this step takes less than 10 minutes.

 

Note: The time for vacuum-pumping should be less than 3-5 minutes ,otherwise, once the silicone rubber has cross-link reaction during vacuum pumping process, it will not be operated.

 

 

 

Step Three: Pouring the mixture into the frame with original mold slowly . 

 

 

 

Shelf life for silicon rubber for mold making

 

8~10months, when stored in a dry & cool place under the room temperature 25.

 

 platinum catalyst addition cure silicone rubber

 

Packing for platinum catalyst addition cure silicone rubber

 

20kg/drum for part A+ 20kg/drum for part B in one set 

 

,200 kg/drum for part A+ 200kg/drum for part B in one set 

 

 

 

 

 

  

If you have any questions with platinum catalyst addition cure silicone rubber, feel free to contact MS Aimee

 

MSN:aimeezhou055722(at)hotmail(dot)com
Skype: aimee055722

Email:hysz(at)szrl(dot)net
Tel: 0086-755-89948006
Mob: 086-18938867541
Trademanager:cn200039753

 

 

Nearest port for product export
Shenzhen, Guangzhou, Xiamen, Shanghai
Delivery clauses under the trade mode
FOB, CFR, CIF
Acceptable payment methods
T/T, L/C, Westem Union
Export mode
Export through agents
Contact Suppliers

Follow this Suppliers