group nameRTV-2 silicone rubber for molds making
Min Order200 kilogram
brand nameHong Ye silicone rubber
modelRTV-2 silicone rubber,620# ,625#,628#, 728# silico
payment methodT/T, L/C, Westem Union
update timeTue, 05 Nov 2013 11:53:54 GMT
Classification Chemical Auxiliary Agent
Certification SGS,MSDS,RoHS
Sample Free
Transportation by sea or by air
Technical Support Free
Type Silicone Rubber
Application for gypsum molding
HS CODE 3910 0000
Min Order200 kilogram
a. Applications of Condensation silicone for candle moulds
Condensation silicone for candle moulds is mainly used for model design of manual mold, PVC plastic molds, cement products, low melting point alloy molds, alloy toys, plastic toys, electronics, handicrafts, stationery, large-scale sculpture, reproduction of cultural relic, shoe sole molds, pad printing allocation, Electronic equipment antivibration, etc.
b. Operation Instructions for Condensation silicone for candle moulds
Condensation silicone for candle moulds is a flowable liquid, and the quality has nothing to do with the color. It consists of two component. Part A is a flowable liquid silicone rubber, part B is the curing agent. Firstly, after your previous work of dealing with the original model, take some liquid silicone rubber , add 2%-3% curing agent of the amount of silicon, and mix them evenly. Then after vacuum-pumping the mixture, you can pour it into the mold frame. The silicone mold will cured in 2-3 hours.
Note: The time for vacuum-pumping should be less than 3—5 mins ,otherwise, once the silicone rubber has cross-link reaction during vacuumizing, it will not be operated.
FAQ of Condensation silicone for candle moulds
How to prevent silicone manual molds getting sticky?
The main reason for this problem is that you do not handle the products or original molds well, then you should deal with the original mold or products carefully before molding. Such as for the products with a complicated pattern or a unsmoothed surface, you should polish and clean the products after which it will be molded ,then spray the release agent. Normally, the release agent can be Vaseline , detergent. liquid wax Etc. In practical process, you can bush different release agent according to different material.
The second reason is that the operator pour the silicone into the mold when the mixture is mixed evenly, then the finish silicone mold will not cure and dry entirely.