1,000 - 40,000 kilogram
40,001 - 999,999 kilogram
group nameRTV-2 silicone rubber for molds making
Min Order1000 kilogram
brand nameHong Ye silicone rubber
modelHY625# silicone rubber
payment methodT/T, L/C, Westem Union
update timeTue, 05 Nov 2013 12:00:59 GMT
Application Make molds
Color White
Appearance Fluid
Mix ratio 100:3
Low Shrinkage <0.3%
Quality Similar to Smooth On
Package 25kg/drum, 200kg/drum
Delivery time 3 days after payment confirmed
Cerficate Rohs, ISO 9000:2001
Shelf life 12 months
Min Order1000 kilogram
Condensation Silicone Rubber For Resin Casting is used for
- Polyester resins, epoxy resins, polyurethane resins.
- Polyurethane elastomers.
- Natural and synthetic waxes.
- Plasters and cements.
- Low-melting point
- Imitation wood
Features of Condensation Silicone Rubber For Resin Casting:
- Two-part RTV Silicon rubber:flowable liquid silicon and curing agent.
- Cures at room temperature within 2-4 hours.
- An exceptional fluidity and good operability.
- Temperature and deformation resistance as well as low shrinkage.
- High duplication times
Condensation Silicone Rubber For Resin Casting operations
If the customer wants to make large products and large size molds, the mold should be made of silicon rubber with high hardness. On the contrary, if the mold with fine and precision patterns, it should be made of silicon with low hardness. The amount of the curing agent depends on the actual requirements of the customer. If molds requiring fast drying and demold, more curing agent is needed; contrarily, if molds requiring slower drying and demold, less curing agent is needed.
(Note: our company does not recommend you to add silicone oil. If a special soft silicone mold or fine detailed and complex patterns products are required, 5%-10% silicone oil can be added to soften the mold for easy demold.)
Frequently asked questions of Condensation Silicone Rubber For Resin Casting
Why does the silicone rubber mold have few molding times?
The silicone rubber mold has few molding times is due to follwoing reasons: adding too much silicone oil which will destroy the molecular of silicone rubber; making the mold for small and fine detailed products with higher hardness silicone rubber which is easy to break; making the mold for large products with soft silicone rubber which will reduce the tensile and tear strength of the mold, and the mold will have deformation. Thus, we should take the proper silicone rubber to make the mold for suitable products.