Molding Silicon Rubber Pouring with 40 shore A

FOB Price
  • US $7.80

    200 - 40,000 kilogram

  • US $5.80

    40,001 - 999,999 kilogram

  • group nameRTV-2 silicone rubber for molds making

  • Min Order200 kilogram

  • brand nameHong Ye silicone rubber

  • modelcondensation molding silicon rubber 640#

  • payment methodT/T, L/C, Westem Union

  • update timeTue, 05 Nov 2013 12:28:08 GMT

Paramtents

  • color adjustable

  • condition liquid

  • application make molds for big size

  • mixing ratio 2-3%

  • purity 100%

  • sample available

Packging & Delivery

  • Min Order200 kilogram

Briefing

Pouring Molding Silicon Rubber Advantages:
Low shrinkage;
Favorable tension.

Detailed

Molding Silicon Rubber Pouring with 40 shore A

  • Applications:

Pouring Molding Silicon Rubber 640# with the hardness of 38-42 shore A, is specially suitable for large crafts mould making and duplication of poly resin crafts in pouring way, PU crafts, gypsum or plaster, unsaturated resin, lighting and candles crafts, plastic toy, stationery gifts crafts, large statue buddha, furniture decoration, cement, articficial stone, etc.

 

  • Advantages : light viscosity, pourable effort, good fluidity, easy-operation, good tension and high tear strength.

 

  • Features:

Model

Viscosity

(cps)

Hardness

(Ao)

Tensile Strength (Mpa)

Tear Strength (KN/m)

Elongation

(%)

Mixing ratio (%)

Operating Time(H)

Curing Time(H)

640

≤10000

38+/-2

≥3.0

≥16

≥260

2-3

0.5-1

2-5

 

  • FAQ:

Why is the silicone rubber mold oily?

Basically, molding silicone rubber doesn't contain any oil, so it won't be oily. The reasons for the oily molds can be deducted from the below 3 factors:

1. Added white oil, which is the compound of silicone oil and white oil. The white oil is not silicone oil but a kink of petrochemicals;

2. Added too much silicone oil. Normally, we donot advise our customers to add any silicone oil into silicone rubber. If necessary, the ratio must be 5%-10%;

3. Added too much curing agent, this is another reason for oily mold.

 

Further information, please feel free to contact Firleanna:

SKYPE:HY-Firleanna

T: 86-755-89212365

M:86-18938867520

F: 86-755-89948030

3w(dot)szrl(dot)net

3w(dot)sellsilicon(dot)com

Nearest port for product export
Shenzhen, Guangzhou, Xiamen, Shanghai
Delivery clauses under the trade mode
FOB, CFR, CIF
Acceptable payment methods
T/T, L/C, Westem Union
Export mode
Export through agents
Contact Suppliers

Follow this Suppliers