Price Molding Silicone HOT!

FOB Price
  • US $7.87

    200 - 40,000 kilogram

  • US $5.23

    40,001 - 999,999 kilogram

  • group nameRTV-2 silicone rubber for molds making

  • Min Order200 kilogram

  • brand nameHong Ye silicone rubber

  • modelRTV630#

  • payment methodT/T, L/C, Westem Union

  • update timeTue, 05 Nov 2013 13:21:28 GMT

Paramtents

  • color white

  • certifications RoHS.MSDS.SGS

  • operation way brushing

  • hardness 30shore A

  • shrinkage low shrinkage

  • visicosity low visicosity

  • deformation no deformation

  • elasticity good elasticity

  • duplication times 800-1000

Packging & Delivery

  • Min Order200 kilogram

Briefing

Price Molding Silicone
competitive price with high quality
light viscosity
4% free catalyst
SGS,Rosh,ISO9001:2000

Detailed

Description of Molding Silicone

 

Molding Silicone are used by thousands of sculptors and foundries for casting concrete and other sculpture materials to make accurate reproductions of original sculpture.molding silicone rubber can be poured on , brushed on to any original sculpture and will reproduce detail perfectly. reproductions can be cast in urethane plastic, epoxy resin, plaster, concrete, and more.

 

 

Price Molding Silicone HOT!  

 

Features of  Molding Silicone 

 a.low viscosity

 b.easy operation

 c.long shelf life over 12 months

 d.good tear strength and low shrinkage

 e.curing at room temperature within 2-4hours

 f.high duplication times and no deformation

 

Price Molding Silicone HOT!

   

Technical datasheets of  Molding Silicone 

 

Model

Our625#

A/B

Dow Coring

E3481

Smooth-on

Mold Max ® 25T

Mixing proportion of catalyst(%)

100:4

100:5

100:5

Hardness (A°)

23~25

21~25

25

Comparison based on 25 Shore A

Density ( g/cm3 )

1.12

1.20

1.18

Viscosity (25 C°,mPa.s)

19,000

25,000

25,000

Tensile strength (Mpa)

≥3.0

4.0

4.0

Tear-strength (KN/m )

≥25

23

23

Elongation-break(%)

≥ 400

370

375

Working time (minutes)

30~60

90~120

45

Curing Time (hours)

12~24

24

24

Liner shrinkage (%)

0.3

0.2~0.5

0.2

 

 

FAQ of Molding Silicone

Why does the silicone mold get burnt out?

This consequence happens only because you have left out the important notes when using unsaturated resin materials to produce your products. The unsaturated resin produces great heat when added the curing agent. So you must demould the product within 3 minutes to avoid this problem.

 

Price Molding Silicone HOT!

 

 

Any questions about Silicone Rubber, Leah is at your service.

TEL: 086-755-89212382

FAX: 086-755-89948030

MOBILE: 086-189 3886 7561

Website: www(dot)szrl(dot)net

E-MAIL: hyji(at)szrl(dot)net

Skype: leahchou1214

QQ: 189 3886 7561

Nearest port for product export
Shenzhen, Guangzhou, Xiamen, Shanghai
Delivery clauses under the trade mode
FOB, CFR, CIF
Acceptable payment methods
T/T, L/C, Westem Union
Export mode
Export through agents
Contact Suppliers

Follow this Suppliers