200 - 40,000 kilogram
40,001 - 999,999 kilogram
group nameRTV-2 silicone rubber for molds making
Min Order200 kilogram
brand nameHong Ye silicone rubber
model625#
payment methodT/T, L/C, Westem Union
update timeFri, 08 Nov 2013 14:08:44 GMT
Color White
Mixing ratio 100:4
Catalyst 4% for free
Shelf life 12 month
Hardness Shore A 25
Packing 25kg/pail
Payment T/T
Certification REACH,ROHS,ISO
Feature High duplication times rubber
Characteristic High tear and tensile strength
Min Order200 kilogram
High strength silicone rubber for molding
Mainly application of High strength silicone rubber for molding
High strength silicone rubber kit,rubber kit,silicone kit,moldmaking kit is a two part silicone rubber and curing with tin catalyst. As with a low viscosity, high strength and excellent duplication times.
High strength silicone rubber for moldingwidely used for
concrete casting
cement products casting
making silicone molds for artificial stone
concrete statue molds,garden statue molds
stone molds
cement crafts
GRC/GPR decorations,ect.
Features of High strength silicone rubber for molding
a.low viscosity
b.easy operation
c.long shelf life over 12 months
d.good tear strength and low shrinkage
e.curing at room temperature within 2-4hours
f.high duplication times and no deformation
How to make a silicone mold with High strength silicone rubber for molding
a. clear and smooth original moulds
b. brush on release agent
c. correct weigh accoring to the mixng ratio
d stir the two parts evenly
e. vacuum-pumping less than 10min
f. pouring or brushing
(Note: We are not recommend you to add silicone oil. If a special soft silicon mold or fine detailed and complex patterns products are required, 5%-10% silicone oil can be added to soften the mold for easy demould.)
Frequently asked questions of High strength silicone rubber for molding
Why does the silicone rubber mold have few molding times?
The silicone rubber mold has few molding times is due to follwoing reasons: adding too much silicone oil which will destroy the molecular of silicone rubber; making the mold for small and fine detailed products with higher hardness silicone rubber which is easy to break; making the mold for large products with soft silicone rubber which will reduce the tensile and tear strength of the mold, and the mold will have deformation. Thus, we should take the proper silicone rubber to make the mold for suitable products.
Why does the silicone mold get burnt out?
This consequence happens only because you have left out the important notes when using unsaturated resin materials to produce your products. The unsaturated resin produces great heat when added the curing agent. So you must demould the product within 3 minutes to avoid this problem.
For getting further information about RTV-2 silicone rubber, PLS contact with
Ms Moe
Email: hyt(at)szrl(dot)net
Skype: moe.chai
Tel: 86-755-89948019
Mob: 86-18938867514
Web: ..........net
TDS of High strength silicone rubber for molding
Model | 638# | 630# | 625# | 620# |
Appearance | white | white | white | white |
Mixing proportion of curing agent (%) | 5% | 5% | 5% | 5% |
Operating time (mins 25 0C ) | 40~70 | 60~90 | 40~70 | 30~50 |
Curing time(hours 25 0C) | 4~7 | 5~7 | 4~7 | 3~5 |
Hardness (A°) | 36±2 | 30±2 | 25±2 | 20±2 |
Viscosity (Mpas -25 0C) | 30000~38000 | 27000~32000 | 17000~19000 | 12000~14000 |
Tensile-strength(Mpa) | ≥4.50 | ≥4.2 | ≥3.2 | ≥2.8 |
Tear-strength (KN/m) | ≥30 | ≥30 | ≥27 | ≥32 |
Elongation-break(%) | ≥ 420 | ≥ 440 | ≥ 440 | ≥ 420 |
Linear Shrinkage (%) | ≤0.3 | ≤0.3 | ≤0.3 | ≤0.3 |
网络文化经营许可证:浙ICP备14006100号-11 2007-2024 Tradevv.com. All rights reserved.