200 - 40,000 kilogram
40,001 - 999,999 kilogram
group nameAddition cure silicone rubber
Min Order200 kilogram
brand nameHong Ye silicone rubber
modelEM625#
payment methodT/T, L/C, Westem Union
update timeFri, 08 Nov 2013 17:23:36 GMT
Color Adjustable
Certificate SGS,RoHS,ISO
Hardness of silicone 25 A°
Application size of mold small/ medium
Recommend operation way pouring/brushing
Retractility(%) ≤0.25
Application moldmaking/molding
Shelf life 12 months
MOQ 200KG
Sample available
Min Order200 kilogram
rtv silicone for molds making
Appilication of rtv silicone for molds making
Emax Brand rtv silicone for molds making is primarily intended for the reproduction of plate engrave ,human replica,for the mold making of poly resin crafts, PU crafts, PU resin crafts,gypsum crafts ,unsaturated resin crafts, lighting and candles crafts ,soap mold,plastic toy , stationery gifts crafts industry, a large statue Buddha, furniture, furniture decorative materials, statues Buddha, artifacts copied, building decoration materials, large-scale cement mold, artificial fossils Factory, Europe component factory, simulation landscapes, animals and plants sculpture, sandstone crafts and so on.
rtv silicone for molds making features description
Emax silicone is white or red flowing liquid with general hardness of 22-50A°after curing. Hongye mold making liquid silicon rubber is a kind elastic silicon rubber mold which features with resistance to deformation, high-temperature, acid-alkali and expansion as well as high reproduction times, good tensile strength, tear strength and elongation.
rtv silicone for molds making operations
If the customer wants to make large products and large size molds, the mold should be made of silicon rubber with high hardness. On the contrary, if the mold with fine and precision patterns, it should be made of silicon with low hardness. The amount of the curing agent depends on the actual requirements of the customer. If molds requiring fast drying and demold, more curing agent is needed; contrarily, if molds requiring slower drying and demold, less curing agent is needed.
(Note: our company does not recommend you to add silicone oil. If a special soft silicone mold or fine detailed and complex patterns products are required, 5%-10% silicone oil can be added to soften the mold for easy demold.)
mold silicone rubber for candle mold reproduction
Frequently asked questions of rtv silicone for molds making
Why does the silicone rubber mold have few molding times?
The silicone rubber mold has few molding times is due to follwoing reasons: adding too much silicone oil which will destroy the molecular of silicone rubber; making the mold for small and fine detailed products with higher hardness silicone rubber which is easy to break; making the mold for large products with soft silicone rubber which will reduce the tensile and tear strength of the mold, and the mold will have deformation. Thus, we should take the proper silicone rubber to make the mold for suitable products.
Why does the silicone mold get burnt out?
This consequence happens only because you have left out the important notes when using unsaturated resin materials to produce your products. The unsaturated resin produces great heat when added the curing agent. So you must demould the product within 3 minutes to avoid this problem.
CERTIFICATION:
ISO9001: HK05/01358
SGS:GZ0606100461/CHEM
RoHS:BTRS091718751
Patent:ZL200520001597.8
Delivery terms:FOB,CFR,CIF
Exchange rate:1USD=6.30RMB
Packing:5kg/pail,25kg/pail,200kg/pail
Delivery time is within 3 days after getting your bank receipt.
Payment Terms: T/T 100% in advance,L/C,Western Union
Mind order quantity(MOQ):200KG
Transport: by sea or by air
Shelf life:12 months under room temperature not open
Any further information of modling silicone rubber required or suggestion, pls feel free to call
Ms. Moe
T*el:86-18938867514
M*ail:hyt(at)szrl(dot)net
Welcome to our website for further information www dot szrl dot net
网络文化经营许可证:浙ICP备14006100号-11 2007-2024 Tradevv.com. All rights reserved.