100 - 40,000 kilogram
40,001 - 999,999 kilogram
group namePad printing silicone rubber
Min Order100 kilogram
brand nameHong Ye silicone rubber
model901# 902# 912# 916# 918# pad printing silicone wi
payment methodT/T, L/C, Westem Union
update timeSat, 09 Nov 2013 11:36:00 GMT
Color white, red , green, yellow
application for pad printing
shelf life 12 months
packing vacuum pumping
MOQ 200 kg
delivery within 3 days after payment
mixing ratio 100:3
operation time 30-40 mins
curing time 3-4 h
payment terms T/T, L/C
Min Order100 kilogram
Usages of pad printing silicone rubber with good resilience
pad printing silicone rubber with good resilience is mainly use for printing irregular patterns of plastic toys, electroplating toys and trade makers . Pad printing silicone rubber as a carrier which transfer patterns on the steel plate to the toys products surface.
Features of pad printing silicone rubber with good resilience:
pad printing silicone rubber with good resilience with high print times and abrasion resistance. Pad printing silicone rubber has good printing effects, permanent and durable. We can provide all kinds of color and our catalyst is free.
Instructions of pad printing silicone rubber with good resilience:
pad printing silicone rubber with good resilience is two-component silicone, part A is liquid silicon rubber, part B is catalyst. The usual mixture of silicone rubber and catalyst is 100: 2 or 100: 3. E.g. we take 100g of liquid silicon rubber and 2g-3g catalyst, mix them and pour it to your mold. A fter 2-4 hours, you will get a Pad printing silicone rubber.
FAQ of pad printing silicone rubber with good resilience
Why the pad printing silicone rubber with good resilience is incomplete or not clear?
a. If the silicon pad is too hard while the pattern is very delicate or small, the printing patterns will be incomplete or not very clear, for in that way the silicon pad could not adsorb the printing ink from the steel plate well. If your pattern is very delicate or small, please use soft silicon pad for pad printing.
b. If the percentage of water in the ink is very high, the printing pattern also will be incomplete, and spot may appeared. For this situation, please clean your ink box, or change the printing ink or Tianna water.
For getting further information about pad printing silicone rubber with good resilience, PLS contact with Miss Caroline
TEL: +86-755-89948019
Mobile: +86-18938867567
Skype: cathy19900719
Email: hysf(at)szrl(dot)net
Website : www(dot)szrl(dot)net
网络文化经营许可证:浙ICP备14006100号-11 2007-2024 Tradevv.com. All rights reserved.