Pad printing silicone for stamping picture

FOB Price
  • US $14.78

    200 - 40,000 kilogram

  • US $8.95

    40,001 - 999,999 kilogram

  • group namePad printing silicone rubber

  • Min Order200 kilogram

  • brand nameHong Ye silicone rubber

  • modelHY 918

  • payment methodT/T, L/C, Westem Union

  • update timeSat, 09 Nov 2013 11:36:19 GMT

Paramtents

  • Color half transparence

  • Hardness 26~30 Shore A

  • Proportion of picture and pad 1:3

  • Certifications ISO,RoHS,SGS,FDA

  • sample avaliable

Packging & Delivery

  • Min Order200 kilogram

Briefing

high tensile & tear strength ,Low linear shrinkage,Reasonable price ,free Curing agent

Detailed

1. Pad printing silicone rubber 918# datasheet:

Model 

Appearance 

Viscosity (cps) 

Hardness (Ao) 

Tensile Strength (Mpa) 

Tear Strength (KN/m) 

Elongation (%) 

Mixing Ratio(%) 

918

red / yellow 
/ green / white

28000~34000

28±2

≥3.6

≥2.6

≥420

2~3

 

 

Pad printing silicone for stamping picture 

 

2. Pad printing silicone rubber application:

 

- Pad printing is primarily used for non-uniform, multidimensional products like a golf ball. Flat surfaces can be pad printed as well.
- Typical image sizes are less than 3" in diameter, but print sizes of 5" or larger can be achieved in special occasions.
- You can pad print a very wide range of substrates, including plastics, metals, glass, ceramic, vinyl, rubber, polypropylene, leather, acrylic, cotton, even food items and more. A pad printer is NOT a documentation printer but it can be used for printing on paper products, for instance paper cubes or napkins.

.

 

4.Frequently asked question of pad printing silicone rubber:

  Why the printed pattern is incomplete or not clear?

--If the silicon pad is too hard while the pattern is very delicate or small, the printing patterns will be incomplete or not very clear, for in that way the silicon pad could not adsorb the printing ink from the steel plate well. If your pattern is very delicate or small, please use soft silicon pad for pad printing.

---If the percentage of water in the ink is very high, the printing pattern also will be incomplete, and spot may appeared. For this situation, please clean your ink box, or change the printing ink or Tianna water. 

 

Any questions,please feel free to contact Ms. Moe:

Mob: +86-18938867514

FAX: 086-755-89948030

 

 

 

Nearest port for product export
Shenzhen, Guangzhou, Xiamen, Shanghai
Delivery clauses under the trade mode
FOB, CFR, CIF
Acceptable payment methods
T/T, L/C, Westem Union
Export mode
Export through agents
Contact Suppliers

Follow this Suppliers