100 - 40,000 kilogram
40,001 - 999,999 kilogram
group namePad printing silicone rubber
Min Order100 kilogram
brand nameHong Ye silicone rubber
modelHY625
payment methodT/T, L/C, Westem Union
update timeSat, 09 Nov 2013 11:43:33 GMT
Application pad printing silicone rubber
H.S. code 39100000
Appearance Liquid
Purity 100%
MOQ 100kgs
Sample Free
Package Vacuum packing
Cetificate FDA,SGS, RoHS, MSDS, ISO9001:2000
Port shenzhen
Min Order100 kilogram
pad printing silicone
Key words: pad printing silicone rubber, rtv silicone, pad printing silicone, liquid silicone for pad printing, silicone for pad printing, liquid silicone for printing.
Characteristics of pad printing silicone
pad printing silicone is a double-component silicone rubber, and can be vulcanized in room temperature. Solidify time depends on the mount of curing agent, the more the curing agent, the faster the curing.
Application of pad printing silicone:
pad printing silicone isapplicable to plastics toys, electroplating products, PVC toys, plastics toys, craftworks, trademarks and irregular pattern printing .it has the advantage of abrasion resistance, high temperature resistance, good printing effect, etc.
Features of pad printing silicone:
a) Resistance to deformation, high-temperature
b) High printing times
c) Good aging resistance
d) Exceptional elasticity
e) Great printing effect
Usage ofpad printing silicone:
1) Uniformly stir the silicone rubber for pad printing for 5-10 minutes in the package barrel before use.
2) Clean the mold with detergent, and dry up the mold by a piece of cloth or an air gun and then coat the mold with a layer of release agent.
3) The normal proportion between the printing silicone and si-oil depends on the requirements of the customers. If pattern is too big, a soft silicon pad is needed and the amount of si-oil is increased. Contrarily, if a silicon pad with high hardness is needed, the silicone oil should be added less or not. The appropriate hardness of general pad printing silicone rubber is 15A°~-25 A°; if too much silicone oil is added, the silicon pad is so soft that the printing times is limited, thereby bringing about abrasion intolerance, solvent intolerance and ageing
FQA of pad printing silicone:
:
·Why is the pad printing siliconenon-durable are?
1.Because of the imcompleted process of filtering , there are some impurities left in the pad printing silicon rubber .
2.As we know, silicon oil is a additive which will destroy the molecular chain of the silicon rubber for pad printing then it will cause the easy ageing .
3.some customers don’t change the printing pad according to the size of the pattern , for large pattern, large silicon pad should be used ,otherwise ,use small one .
Any question abt pad printing siliconeplease feel free to ask Cindy:
Tel: 86-755-89948158
Mob: 86-13266634823
Email:hysg(at)szrl(dot)net
Skype:cindyyeah5
Msn: hycdy(at)live(dot)cn
网络文化经营许可证:浙ICP备14006100号-11 2007-2024 Tradevv.com. All rights reserved.