Amorphous Ribbon is an new soft magnetic material.
It has the common material property of soft magnetic, like low coercivity(Hc), high saturaion flux density(Bs), low loss(Ps), and high stability.
New Soft MagneticSolution
Amorphous aremainly used to replace silicon sheet:
Amorphous canreduce the fe-loss by 60-70%
Work frequencybetween 50Hz to 10KHz
Lowerloss: 1/3 to 1/5 of silicon sheet
Energy-savingseries of amorphous transformer
Amorphous motor
Pure electricvehicles
Charging piles
Photovoltaicmaterial
Material forsubmarine with high strength and corrosion resistance to salt water
Energy saving andemission reduction of urban tram
1K101 amorphous ribbon parameter between Zhongyueand Hitachi
Comparison of 1K101 amorphous ribbon magnetic properties |
1K101 | | Bs/T | Br/T | Hc/(A/m) | Ss/(W/kg) | Ps/(VA/kg) |
Zhongyue | Before annealing | 1.08 | 0.8 | 3.91 | 1.33 | 0.45 |
Hitachi | 1.01 | 0.75 | 5.76 | 2.4 | 0.32 |
Zhongyue | After annealing | 1.56 | 1.21 | 2.09 | 0.2 | 0.15 |
Hitachi | 1.56 | 1.13 | 1.93 | 0.072 | 0.11 |
Saturation induction density Bs /T | 1.56 | Saturation magnetostriction constant λs | 27*10-6 |
Curie temperature Tc(℃) | 410 | Density d(g/cm3) | 7.18 |
Crystallizing temperature Tx(℃) | 535 | Electrical resistivity ρ(Ωm²/m) | 130 |
Hardness HV(kg/mm2) | 960 | Coercive force Hc(A/m) | <4 |
specification | Bandwidth (mm) | Thickness (μm) | Thickness deviation (μm) | Lamination factor |
spray tape 1K101 | 2-220 | 25 | ±2 | >0.80 |
2-220 | 25 | ±2 | >0.75 |
Shear tape 1K101 | 2-220 | 25 | ±2 | >0.80 |
2-220 | 25 | ±2 | >0.75 |
All the specifications canmake customized requirements, and we provide live guidance for your producetechnique.