200 - 40,000 kilogram
40,001 - 999,999 kilogram
group nameelectronic potting silicone rubber
Min Order200 kilogram
brand nameHong Ye silicone rubber
modelHY9055#
payment methodT/T, L/C, Westem Union
update timeFri, 08 Nov 2013 19:33:55 GMT
color white
certifications RoHS.MSDS.SGS ISO9001:2000
operation way pouring
hardness 55 shore A
Mixing Ratio 1:1
Viscosisty(after mixing) (cps) 2000~3000
Curing time1 (min, 25degree) 120
Curing time 2 (min, 25degree) 480
MOQ 200kg
Min Order200 kilogram
Features & Applications of Silicone for LED encapsulation
Silicone for LED encapsulation is condensation silicone potting compound in two parts with low viscosity.
It can be cured completely at room temperature. It works on the surface of material as PC(Poly-carbonate),PP,ABS,PVC as to its superior bonding feature. It is also applicable for insulation, waterproof and bonding of electronics parts. It meets the requirements of European RoHS.
Typical Application of Silicone for LED encapsulation
- Potting for Protetion of general electronic Module.
- Outdoor protection for LED screen.
TECHNICAL GUIDELINES of Silicone for LED encapsulation
1, Pls put part A and part B in separate container and stir evenly before mixing the two parts together.
2, Weight Ratio: part A: part B = 10:1
3, Bubble release if necessary. Desecration the mixture under 0.08 MPa for 3 minutes.
4, HY 210 is cured at room temperature, so pls put it under room temperature after pouring. It comes to next process when basically cured, and it takes about 24 hours for completely cured.
Kindly note: Temperature and Humidity with tremendous influences for curing of HY 210.
Warm Tips of Silicone for LED encapsulation:
1. Sealing package for storage. The mixture should be used up at once to avoid wasting.
2. Silicone belongs to non-dangerous goods, but keeps away from mouth and eyes.
3. When it gets stratified after a period of storage, please mix it evenly before using, it does not affect the performance.
Silicone Potting Compound technical guidelines:
1, Pls put part A and part B in separate container and stir evenly before mixing the two part together.
2, Mixing Ratio: part A: part B = 1:1
3, Deaeration the mixture in vacuum pump under 0.08 MPa for 3-5 minutes.Then the mixture could be used for pouring.
Any questions about Silicone Rubber, Leah is at your service.
TEL: 086-755-89212382
FAX: 086-755-89948030
MOBILE: 086-189 3886 7561
Website: www(dot)szrl(dot)net
E-MAIL: hyji(at)szrl(dot)net
Skype: leahchou1214
QQ: 189 3886 7561
网络文化经营许可证:浙ICP备14006100号-11 2007-2024 Tradevv.com. All rights reserved.